Cracks are almost always present
Nearly every concrete slab on Guam has some cracking within a few years of the pour. Concrete shrinks slightly as it cures, and slabs move with temperature and ground moisture. A hairline crack by itself is not news. What matters is the pattern, the width, and whether it is changing.
What a normal crack looks like
Shrinkage cracks are thin — often thinner than a credit card — straight or gently curved, and do not step up or down across the crack line. They usually appear within the first year, especially near corners, door openings, or anywhere the slab is a different thickness. They do not widen over time and there is no vertical offset when you run a hand across them.
What's worth a second look
A crack wider than about 1/8 inch, one where you can feel a lip or step between the two sides, or one that runs diagonally from the corner of a window or door and keeps getting longer, is a different category. So is a crack that lets water track through to a lower level, or one paired with a door or window that has started sticking. Those point to settlement — the ground under part of the slab moving — rather than ordinary shrinkage.
Guam-specific causes
A lot of settlement on the island traces back to fill soil that was not compacted properly before the original pour, or to water finding its way under a slab edge over years of rain and eroding the base from beneath. Older homes built before current compaction standards were consistently enforced are more likely to show this than recent construction.
What we do about it
For shrinkage cracks, the fix is usually cosmetic — routing and sealing the crack to stop water and debris getting in, nothing more. For settlement, we dig to find out what is actually happening under the slab before proposing a fix, because patching the surface over a soil problem does not last. If you are not sure which one you are looking at, send a photo with a coin or a tape measure next to the crack for scale — that is usually enough to tell from here.